03 — Selection & applications
(a) Chemically aggressive media
The corrosion case is the family's strongest: concentrated acids and
alkalis, permanent seawater submersion (smbbearings.com). The Etor
comparison (published 2026-03-08) claims ceramic ball bearings "can
last up to three times longer than stainless steel bearings in chemical
plant applications" — a vendor claim, and flagged as such, but the
mechanism (no electrochemical corrosion at all) is material fact.
Plating, chemical dosing, pickling and marine-submerged duty are the
canonical cases.
(b) Extreme temperature, both directions
The −210 °C to 800 °C range is SMB's published figure for its uncaged
Si3N4 execution, not a general rating for every full-ceramic assembly.
The same manufacturer gives distinct ceilings: full-complement
Si3N4 can reach 1200 °C only at low speed and very low axial load;
PEEK-cage versions are rated up to 250 °C; 316 stainless-cage versions
up to 500 °C. Below −70 °C, SMB suggests considering PTFE or 316 cages,
but does not publish a numeric minimum for those caged variants.
PEEK/PTFE retainers or seals limit the maximum to approximately 250 °C.
These figures must be read with the exact bearing's load, speed,
clearance and lubrication data. A material's temperature window does
not establish the operating envelope of a complete bearing, and
oil-free running must be confirmed for the selected execution.
(c) Non-magnetic and insulating duty
The ISK guide lists "anti-magnetic and electrically insulating
properties" among the material's core characteristics; the Talos
comparison adds medical MRI and vacuum process equipment as the classic
applications. An all-ceramic bearing neither magnetizes nor conducts —
relevant where either property contaminates the measurement or the
product.
(d) When full ceramic is NOT the answer
Shock: the Yuan He comparison is unambiguous — steel deforms under
overload, ceramic cracks; unpredictable shock loads default to steel.
Speed at load: full-ceramic zirconia runs ~20% of stainless speed; the
fast answer is hybrid Si3N4 balls. And budget: at 10–50× steel cost,
a duty that 440C stainless survives (moisture, washdown, mild
chemicals) should stay stainless. Step to full ceramic only when the
duty defeats the metal ladder — that is the family's honest scope.